    地面找平怎样才能不开裂?
    来源:http://www.jndmzp.com   时间:2020-9-1 14:29:44
    在我们房屋装修中,地面找平是不可少的一个装修工程,我们都知道地面找平不好,就会不好贴砖,会影响项目的顺利进行。那么地面找平应该怎么找平呢?
    In our house decoration, the ground leveling is an indispensable decoration project. We all know that if the ground leveling is not good, it will not be good for tiling, which will affect the smooth progress of the project. How should the ground be leveled?
    说到地面找平,相信大部分的人就会说,就用一些水泥和砂搅拌然后就倒下去铺平一下,也就水泥砂浆地面找平,可是大家知道水泥砂浆地面找平后,它存在大量的缺陷,如厚度厚、粉化起沙、裂纹等。下面就一起来了解一下地面找平应该怎么办。
    When it comes to floor leveling, I believe most people will say that they just mix some cement and sand, then pour it down and pave it, that is, cement mortar floor leveling. But we all know that after the cement mortar floor is leveled, there are a lot of defects, such as thick thickness, powdered sand, cracks, etc. Now let's learn how to do the ground leveling.
    水泥砂浆找平是过去和现在采用较多的一种找平方式,但是存在很多缺陷。
    Cement mortar leveling is the most used square finding method in the past and now, but there are many defects.
    1、找平厚度太厚,水泥砂浆地面找平的厚度在25-35mm左右,如果自建房的高度不是很高,在做了找平处理以后,可能会觉得它的高度更矮,甚至会觉得有些压抑。
    1. The leveling thickness is too thick. The leveling thickness of cement mortar floor is about 25-35mm. If the height of self built house is not very high, after leveling, you may feel that its height is lower, and even feel a little depressed.
    2、如果水泥砂浆配比不对,会使面层粉化起砂,起灰及裂纹。地板(复合地板)与找平层形成一些间隙,人踩上去以后压迫地面灰尘向四周分散,然后从伸缩缝窜出,透过踢脚板缝隙扩散出来,形成了扬灰的现象。

    2. If the ratio of cement mortar is not correct, the surface will be powdered, dusted and cracked. There are some gaps between the floor (composite floor) and the leveling layer. When people step on it, the dust on the ground is pressed to disperse around, and then it comes out from the expansion joint and diffuses through the gap of the skirting board, forming the phenomenon of dust rising.

         

    3、水泥砂浆找平不细致的地方会出现空鼓现象。如果地面没有充分用水打湿,就会造成水泥沙浆的水分被快速吸收。地面的污渍、灰尘过多,水泥沙浆与地面就会很难连接在一起,很容易导致地面空鼓。
    3. There will be hollowing in the place where the cement mortar is not leveled carefully. If the ground is not wet with enough water, the water in cement mortar will be quickly absorbed. If there are too many stains and dust on the ground, it will be difficult to connect the cement mortar with the ground, which will easily lead to the hollowing of the ground.
    4、如果地面水泥砂浆找平不恰当,还会把地面线管破坏。地面找平一定要安排在电路改造结束以后。倘若电线还没有被电工固定好,泥工就开始倒砂浆,地面的线管很容易移位,若是后期铺设实木地板,在实木地板打钉的时候,可能会钉到移位的管子。
    4. If the ground cement mortar leveling is not appropriate, the ground line pipe will be damaged. The ground leveling must be arranged after the circuit transformation. If the wire has not been fixed by the electrician, the plasterer will start pouring mortar, and the pipeline on the ground is easy to shift. If the solid wood floor is laid later, the displaced pipe may be nailed when the solid wood floor is nailed.
    地面起砂的原因很多,水泥沙子配比失衡,重物来回碾压,使用的频率和风化等原因造成的。
    There are many reasons for sand rising on the ground, such as imbalance of cement sand ratio, heavy rolling back and forth, frequency of use and weathering.