    济南自流平存在问题——自流平地坪工程面涂层美观,高洁净、高耐磨和载重,主要的还是美观装饰效果,因为人的视觉反应的就是表面的颜色和表面的效果。自流平地坪工程面涂层质量弊病有:缩孔、花斑、花纹、色差、浮色、变色、露底、咬底、发白、拉丝、无光、脱落、发黏、起油、桔皮等质量问题。以下是所有自流平地坪工程表面质量弊病的形态。

    济南地面找平http://www.jndmzp.com

    Jinan self leveling problems, self leveling floor engineering surface coating appearance, high cleanness, high wear resistance and load, the main or beautiful decorative effect, because of people's vision of the first reaction is surface color and surface effect. Self leveling floor engineering surface coating quality defects: shrinkage hole, piebald, pattern, color, floating color, discoloration, grinning, bite the end, white, drawing, no light, fall off, sticky, oil, orange peel and other quality problems. The following is the surface quality of all self leveling floor surface quality ills of the form.
    1、自流平地坪面涂缩孔:涂料表面张力与底材表面张力相关大、涂料流动性或流平性差、底材表面有油污或水、涂料中消泡剂太多常造成缩孔。
    1, self leveling floor surface coating shrinkage: related coating surface tension and substrate surface tension, coating liquidity or leveling, bottom surface material with oil or water, paint antifoaming agent is too much often cause shrinkage.
    2、自流平地坪面涂花斑:色漆中颜料分散不均匀,调色时色浆混合不充分、分散剂量不准、稀料的溶解性差容易造成花斑现象。
    2, self leveling floor surface is coated with a piebald: paint pigment dispersion is not uniform, color mixed color paste is not sufficient, scattered dose not, thinner poor solubility is easy to cause the piebald phenomenon.
    3、自流平地坪面涂花纹:原因大致与花斑一样,但由于流平性、施工方法上有些差别形成不同的形状。
    3, self leveling floor surface coated pattern: the reason is roughly and piebald like, but due to the flow of the flat, the construction method of some differences in different shape.
    4、自流平地坪面涂色差:批次之间色调不匀、涂层厚度不均匀、涂层涂布时间差大,容易形成色差。
    4, self leveling flat surface Tu color: the color between the batches of uneven, the thickness of the coating is not uniform, the coating time difference, easy to form a color difference.
    6、自流平地坪面涂变色:固化剂选择不当、颜料糊没研磨均匀、颜料选择不对。
    6, self leveling flat surface Tu color: curing agent choice, pigment paste did not grind evenly, pigment choose not.
    7、自流平地坪面涂露底:选用的涂料遮盖力差、使用前易沉降的颜料未被搅起或搅拌不充分、涂料太稀又喷得太薄、底面漆色调反差太大,容易造成露底缺陷。
    7, self leveling floor top coat threadbare: the selection of coating covering power difference, before using easy settling of pigment is not stir up or stirring is not sufficient, coating is too thin and spray too thin, bottom paint color contrast is too big, easy to cause the threadbare defects.
    8、自流平地坪面涂咬底:咬底是上层涂膜喷涂时,涂料中溶剂对底层产生严重的溶胀起皱而脱离的现象。主要是由于底层未干透就涂下一道、底层固化剂量不足、面涂一次喷涂太厚,这些因素会造成咬底现象。
    8. Self leveling flat surface is coated with the bottom: the bottom layer is coated with the upper layer, and the solvent has a serious swelling and wrinkling.. Is mainly due to the underlying unseasoned is painted a, lack of underlying curing dose, painted face a spray too thick, these factors will bite at the end of the phenomenon caused.
    9、自流平地坪面涂发白:作业环境温度太高、溶剂挥发太快、被涂体表面温度过低或环境温度太低、物料或底面中的水分超标等因素易造成发白。
    9, self leveling floor surface coated white: environmental temperature is too high, volatile solvent too fast, is coated body surface temperature too low or the ambient temperature is too low, material or the bottom surface of the water such as excessive factors causing white.
    10、自流平地坪面涂拉丝:涂料的施工粘度太大、雾化性不好、稀料溶解力差、固体份太高、固化剂选择不当速度太快都容易形成拉丝现象。
    10, self leveling floor surface is coated with a drawing: paint viscosity is too large, atomization is not good, thinner dissolved force difference, solids is too high, the curing agent improper selection of speed too fast are easy to form the phenomenon of drawing.
    11、自流平地坪面涂无光:树脂含量过低、涂料细度不合格、溶剂不良、底层太粗糙、环境条件差。
    11, self leveling flat surface coated with no light: the resin content is too low, the fineness of the coating is not qualified, solvent, the bottom is too rough, environmental conditions.
    12、自流平地坪面涂剥落:表面处理不当、底材表面太光滑、涂层相隔时间太久,重涂时没再对表面处理。
    12, self leveling flat surface coating peeling: surface treatment, bottom material surface is too smooth, coating time too long, heavy coating no longer on the surface treatment.
    13、自流平地坪面涂起油:固化剂种类选择不当、溶剂或增柔剂沸点过高及加入比例不对。环氧自流平地坪面涂起泡:起泡是涂膜干燥过程中,滞留于涂膜的气体或反应产生的气体或内部溶剂挥发产生气体强行突破涂膜所留下的痕迹之一。
    13, self leveling flat surface coated with oil: the type of curing agent improper, solvent or increasing the boiling point of the agent is too high and the proportion of the addition is not. Epoxy self leveling floor surface coating blistering: bubble is film drying process, stranded produced in the coating of gas or reactive gas or internal solvent volatilization gas to force a breakthrough one of the traces left by the film.