    关于地平面找平的知识汇总
    来源:http://www.jndmzp.com   时间:2018-12-4 16:14:40
    关于地平面找平的知识汇总
    Summary of Knowledge about Horizon Leveling
    目前空中找平的办法次要有三种:水泥沙浆找平.自流平找平.石膏找平,其中效果好的是自流平找平,但其价位也绝对较高。随着技术的开展,自流平找平技术将会越来越好,价位也会逐步与水泥砂浆找平价钱持平,成爲将来空中找平办法的首选。上面,千水装饰就来给你讲讲在烟台装修中关于空中找平的知识。
    At present, there are three methods of air leveling: cement mortar leveling, self-leveling and gypsum leveling. The best one is leveling, but its price is absolutely high. With the development of technology, the self-leveling technology will be better and better, and the price will gradually be equal to that of cement mortar, which will become the first choice of air leveling method in the future. Above, Qianshui Decoration will tell you about leveling in the air in Yantai Decoration.
    1.空中找平的标准顺序:
    1. Standard order of leveling in the air:
    基层处置→找标高.弹线→洒水潮湿→抹灰饼和标筋→搅拌砂浆→刷水泥浆结合层→铺水泥砂浆面层→木抹子搓平→铁抹子压遍→第二遍压光→第三遍压光→养护
    Base disposal elevation finding. Elastic line sprinkling moisture plastering cake and bar mixing mortar brushing cement mortar bonding layer paving cement mortar surface layer rubbing wood plaster pressing iron plaster for the first time pressing for the second time polishing for the third time maintenance
    2.将基层上的灰尘扫掉,用钢丝刷和錾子刷净.剔掉灰浆皮和灰渣层,用10%的火碱水溶液刷掉基层上的油污,并用清水及时将碱液冲净。
    2. Clean up the dust on the base, brush it with wire brush and chips, remove the mortar skin and ash layer, wash the oil dirt off the base with 10% caustic soda solution, and rinse the alkali solution with clear water in time.
    3.依据墙上的+1000mm程度线,往下量测出面层标高,并弹在墙上。
    3. According to the + 1000mm level line on the wall, the surface elevation is measured downwards and bounced on the wall.
    4.依据房间内周围墙上弹的面层标高程度线,确定面层抹灰厚度(不应小于20mm),然后拉程度线开端抹灰饼(5cm*5cm),横竖间距爲1.5—2.0米,灰饼上立体即爲空中面层标高。假如房间比拟大,还须抹标筋。铺抹灰饼和标筋的砂浆资料配合比均与抹空中的砂浆相反。

    4. Determine the plastering thickness (not less than 20 mm) according to the surface elevation line bounced on the wall around the room, and then draw the beginning of the plastering line (5 cm*5 cm), the horizontal and vertical spacing is 1.5-2.0 meters, and the three-dimensional surface elevation on the gray cake is the air surface elevation. If the room is comparatively large, it needs to be marked with tendons. The mix ratios of mortar materials with plastering cake and standard reinforcement are opposite to those with plastering air.

    济南地面找平

    5.搅拌砂浆,用搅拌机停止搅拌,颜色必需分歧。
    5. Mixing mortar, stop mixing with mixer, color must be different.
    7.铺设水泥砂浆前,涂刷水泥浆一层(随刷随铺面层砂浆)。
    7. Before laying cement mortar, brush one layer of cement mortar (with brush with pavement mortar).
    7.在涂刷完水泥砂浆后,铺水泥砂浆,并在灰饼之间将砂浆铺平均。
    7. After the cement mortar is painted, the cement mortar is laid, and the mortar is evenly laid between the ash cakes.
    8.木抹子刮平后,迅速用铁抹子压遍,直到出浆爲止。面层砂浆初凝后,用铁抹子压第二遍,外表压平压光。在水泥砂浆终凝行进行第三遍压光,必需在终凝前完成。 并随时用2米靠尺反省其平整度。
    8. After scraping the wooden plaster, press it with iron plaster quickly for the first time until pulping. After the initial setting of the surface mortar, press it with an iron plaster for the second time, and smooth the surface. The third calendering of cement mortar during final setting must be completed before final setting. At any time, the flatness is reflected with a 2-meter ruler.
    9.竣工后24小时(空中压光),铺锯末或其他资料掩盖洒水养护,坚持潮湿,养护工夫不少于7天,抗压强度达5Mpa时才干上人。
    9. 24 hours after completion (air calendering), paving sawdust or other information to cover up the sprinkler maintenance, adhere to wet, maintenance time is not less than 7 days, compressive strength of up to 5 Mpa to dry.
    水泥砂浆空中找平验收规范:
    Code for acceptance of air leveling of cement mortar:
    1.水泥砂浆面层与基层应粘结结实,不应空鼓,
    1. Cement mortar surface and base should be bonded, not hollow.
    2.水泥砂浆面层外表应密实压光,不允许有裂痕,脱皮.起沙.接荐不对等缺陷。
    2. The surface of cement mortar should be compacted and compacted, and cracks, peeling, sand lifting and unequal recommendation are not allowed.
    3.不泛水的空中,应按设计要求做好泛水,不得有倒泛水景象。
    3. In the air without flooding, flooding should be done according to the design requirements, and there should be no upside-down flooding.
    4.用2m靠尺反省外表平整度,允许偏向4mm。
    4. Reflect the surface flatness with 2m ruler, and allow the deviation to 4mm.
    综上所述有小马识途地面找平提供,想了解多济南地面找平知识,欢迎关注我们的网站:http://www.jndmzp.com谢谢支持!
    In summary, all the above-mentioned pony ground leveling services, want to know more about Jinan ground leveling knowledge, welcome to pay attention to our website: http://www.jndmzp.com Thank you for your support!