    空中找平不平的弥补方法!
    来源:http://www.jndmzp.com   时间:2018-12-11 14:40:12
    空中找平不平的弥补方法!
    How to make up for the unevenness in the air!
    适用环境:房间平整度略好,空中较爲润滑,部分有不平的中央。
    Applicable environment: The room is slightly smooth, the air is relatively lubricated, part of which has uneven center.
    缺陷:只可用于小范围内的找平运用。
    Defect: It can only be used for leveling in a small range.
    水泥砂浆找平
    Leveling of cement mortar
    优点:这种空中找平办法合适各种空中、各种地板铺设前的空中找平。
    Advantages: This air leveling method is suitable for all kinds of air, all kinds of floors before the air leveling.
    适用环境:房子举架高,暖气片采暖、实木地板铺设前找平、复合地板铺设前找平。
    Applicable environment: the house is elevated, heater heating, solid wood floor leveling before laying, composite floor leveling before laying.
    缺陷:找平厚度太厚在25~35mm,假如水泥砂浆配比不对会使面层粉化起砂,起灰及裂纹。地板(复合地板)与找平层构成一些间隙,易构成扬灰的景象。另外就是水泥砂浆找平不细致的中央会呈现空鼓景象。
    Defects: The leveling thickness is too thick in the range of 25-35 mm. If the proportion of cement mortar is not correct, the surface will be powdered and sand, ash and cracks. The floor (composite floor) and leveling layer form some gap, which is easy to form the scene of raising ash. The other is that if the cement mortar is not leveled carefully, the center will appear empty.
    空中找平要合格规范
    Air Leveling Should Be Qualified and Standardized
    我们普通用2米的靠尺来停止测量,就是说在同一个地位要停止穿插测量,假设测量出来,空隙曾经超越3毫米,那麼阐明空中不平,暂时不能铺地板,找平不合格。普通来说:

    We usually use a 2-meter ruler to stop measurement, that is to say, in the same position to stop the interpolation measurement, assuming that the measurement, the gap has exceeded 3 mm, then clarify the air unevenness, temporarily unable to lay the floor, leveling the unqualified. Generally speaking,

    济南地面找平

    2平方米内落差不超越3毫米的,空中找平合格;
    If the drop within 2 square meters does not exceed 3 mm, the air leveling is qualified.
    2平方米内落差大于3小于5 毫米的,属于空中不平;
    If the drop within 2 square meters is greater than 3 and less than 5 mm, it belongs to the air unevenness.
    2平方米内落差大于5毫米的属于空中严重不平。
    The drop of more than 5 mm in 2 square meters belongs to the serious unevenness in the air.
    空中找平留意事项
    Notices for Air Leveling
    找平后的空中要的是平整度,不要求空中的润滑水平,空中越润滑越容易回潮,反而不好;
    After leveling, the smoothness in the air is needed, and the lubrication level in the air is not required. The more lubrication in the air, the easier moisture regain, the worse it is.
    空中找平常水泥、沙子比例需适宜,找平的空中以不起沙爲好;
    The proportion of ordinary cement and sand in the air should be appropriate, and it is better not to have sand in the air when leveling.
    平整度要求:每2平米之内落差不超越3mm,尤其是走道、门口处应该留意平整度;
    Flatness requirements: every 2 square meters within the drop does not exceed 3 mm, especially in the walkway, doorway should pay more attention to the flatness;
    找平后未干的空中需求留意养护,应该渐渐阴干,避免疾速枯燥;
    After leveling the dry air needs to pay attention to maintenance, should gradually dry, to avoid rapid drying;
    找平后的空中能否枯燥的简易检测办法:找一块40cm以上见方的塑料薄膜,平铺在空中上,周围用物品压严实,次日早上反省,塑料膜上面假如没有分明的水汽、水珠,证明空中枯燥,可以铺装木地板,否则需求持续通风阴干。
    After leveling the air can be boring simple detection methods: find a 40 cm square plastic film, flat in the air, compacted with objects around, the next morning reflection, plastic film above if there is no distinct vapor, water droplets, prove that the air is dry, you can pave wooden floors, otherwise the need for continuous ventilation and drying.
    综上所述有小马识途地面找平提供,想了解多济南地面找平知识,欢迎关注我们的网站:http://www.jndmzp.com谢谢支持!
    In summary, all the above-mentioned pony ground leveling services, want to know more about Jinan ground leveling knowledge, welcome to pay attention to our website: http://www.jndmzp.com Thank you for your support!

鲁公网安备 37148202000237号